Phosphorus-deoxidized UNS C12500 has a copper content of not less than 99.88%.
The following table outlines the mechanical properties of UNS C12500 rods as a function of heat treatment and thickness.
Temper |
Thickness |
Tensile Str. |
Yield Str. |
Elong. |
Rockwell |
Shear Str. |
B |
C |
F |
30T |
M20 |
25.4 mm (1 in) |
221 MPa (32 ksi) |
69 MPa (10 ksi) |
55% |
- |
- |
40 |
- |
152 MPa (22 ksi) |
OS050 |
25.4 mm (1 in) |
221 MPa (32 ksi) |
69 MPa (10 ksi) |
55% |
- |
- |
40 |
- |
152 MPa (22 ksi) |