High-leaded brass UNS C33200 has a copper content of not less than 66%.
The following table shows the mechanical properties of UNS C33200 tubes as a function of heat treatment.
Temper |
Tensile Str. |
Yield Str. |
Elong. |
Rockwell |
B |
C |
F |
30T |
OS025 |
359MPa (52ksi) |
138MPa (20ksi) |
50% |
- |
- |
75 |
37 |
OS050 |
324MPa (47ksi) |
103MPa (15ksi) |
60% |
- |
- |
64 |
26 |
Equivalent materials to UNS C33200 copper alloy are given below:
The chemical composition of UNS C33200 copper alloy is outlined in the following table.
Element |
Content (%) |
Copper, Cu |
65-68 |
Lead, Pb |
1.5-2.5 |
Iron, Fe |
0.07 |
Zinc, Zn |
Balance |