Nov 19 2012
Dispersion strengthened UNS C15750 has a copper content of not less than 98.9%.
The following table shows the mechanical properties of UNS C15750 rod and bar as a function of heat treatment.
Temper |
Tensile Str. |
Yield Str. |
Elong. |
Rockwell |
B |
C |
F |
30T |
M30 |
450MPa (ksi) |
360MPa (52ksi) |
15% |
75 |
- |
- |
- |
|
480MPa (70ksi) |
380 MPa (55ksi) |
15% |
75 |
- |
- |
- |
|
510MPa (75ksi) |
400 MPa (58ksi) |
20% |
80 |
- |
- |
- |