Nov 30 2012
The following table shows the mechanical properties of UNS C50100 tubes as a function of heat treatment.
| Temper |
Tensile Str. |
Yield Str. |
Elong. |
Rockwell |
| B |
C |
F |
30T |
| O61 |
280 MPa (40 ksi) |
80 MPa (11 ksi) |
40% |
- |
- |
- |
35 |
|
225 MPa (32 ksi) |
- |
- |
- |
- |
- |
- |
The chemical composition of UNS C50100 copper alloy is displayed in the following table.
| Element |
Content (%) |
| Tin, Sn |
0.50-0.8 |
| Lead, Pb |
0.05 |
| Fe |
0.05 |
| Copper, Cu |
Remainder |
Copper and the elements mentioned in the above table together constitute 99.5% of this alloy.