Jan 16 2013
UNS C96200 has a copper content of not less than 88.6%.
The following table shows the mechanical properties of UNS C96200 sand cast alloy as a function of heat treatment.
Temper |
Tensile Str. |
Yield Str. |
Elong. |
Fatigue Str. |
M01 |
310MPa (45ksi) |
170MPa (25ksi) |
20% |
- |
|
- |
- |
- |
90MPa (13ksi) |
Equivalent materials to UNS C96200 copper alloy are provided below:
- ASTM B30
- ASTM B369
- MIL V-18436
- QQ C390
- SAE J461
- SAE J462
The chemical composition of UNS C96200 copper alloy is outlined in the following table.
Element |
Content (%) |
Nickel, Ni |
9-11 |
Manganese, Mn |
1.5 |
Iron, Fe |
1.0-1.8 |
Niobium, Nb |
1 |
Silicon, Si |
0.5 |
Phosphorus, P |
0.02 |
Sulfur, S |
0.02 |
Lead, Pb |
0.01 |
Copper, Cu |
Reminder |