Masteel supplies ASME SA387 Grade 22 Class 2 plates to global fabricators who serve the petrochemical, oil, gas and petrochemical industry.
These industries need a pressure vessel grade steel which works well in increased temperatures and this requirement is fulfilled by Masteel’s material. SA387 Grade 22 Class 2 plates have good corrosion and oxidation resistance, making them a good option for sour gas environments as well.
Masteel stocks SA387 Grade 22 carbon alloy plates and can deliver them worldwide.
Equivalents
BS |
EN |
ASTM/ASME |
DIN |
622-515B |
10CrMo910 |
A/SA387-22-2 |
10CrMo910 |
Chromium & Molybdenum content (according to the ASME specification):
Designation |
Nominal Chromium Content (%) |
Nominal Molybdenum Content (%) |
A387 Grade 22 |
2.25% |
1.00% |
Tensile Requirements of Class 2 Plates
Designation |
Requirement |
Grade 22 |
A387 Grade 22 |
Tensile strength, ksi [MPA] |
75 to 100 [515 to 690] |
|
Yield strength, min, ksi [MPa]/(0.2% offset) |
45 [310] |
|
Elongation in 8 in. [200 mm], min % |
|
|
Elongation in 2 in. [50 mm], min, % |
18 |
|
Reduction of area, min % |
45 (measured on round specimen)
40 (measured on flat specimen) |
Chemical Composition of ASME S387 Grade 22 Class 2
. |
. |
Carbon (C) |
% |
Heat Analysis:
Product Analysis: |
0.05 - 0.15
0.04 - 0.15 |
Manganese (Mn) |
% |
Heat Analysis:
Product Analysis: |
0.30 - 0.60
0.25 - 0.66 |
Phosphorus (P) |
% |
Heat Analysis:
Product Analysis: |
0.035
0.035 |
Sulphur (S) (Max) |
% |
Heat Analysis:
Product Analysis: |
0.035
0.035 |
Silicon (Si) |
% |
Heat Analysis:
Product Analysis: |
0.50 max
0.50 max |
Chromium (Cr) |
% |
Heat Analysis:
Product Analysis: |
2.00 - 2.50
1.88 - 2.62 |
Molybdenum (Mo) |
% |
Heat Analysis:
Product Analysis: |
0.90 - 1.10
0.85 - 1.15 |