Nov 23 2012
UNS C35350 leaded brass has a copper content of not less than 61%.
The following table shows the mechanical properties of UNS C35350 rods as a function of heat treatment.
Temper |
Tensile Str. |
Elong. |
Fatigue Str. |
H02 |
445 MPa (64 ksi) |
25% |
175 MPa (25 ksi) |
|
480 MPa (69 ksi) |
- |
- |
|
350 MPa (50 ksi) |
- |
- |
The chemical composition of UNS C35350 copper alloy is outlined in the following table.
Element |
Content (%) |
Copper, Cu |
61 - 63 |
Lead, Pb |
2.0 - 4.5 |
Iron, Fe |
0.4 |
Tin, Sn |
0.3 |
Nickel, Ni |
0.05 - 0.30 |
Phosphorous, P |
0.05 - 0.20 |
Zinc, Zn |
31.3 - 36.2 |