Aluminum bronze UNS C64200 has a copper content of not less than 91.2%.
The following table shows the mechanical properties of UNS C64200 bar as a function of heat treatment and thickness.
Temper |
Thickness |
Tensile Str. |
Yield Str. |
Elong. |
Rockwell |
B |
C |
F |
30T |
M30 |
19 mm. (0.75 in.) |
517MPa (75ksi) |
241MPa (35ksi) |
32% |
77 |
- |
- |
- |
Equivalent materials to UNS C64200 copper alloy are provided in the table below.
ASME SB150 |
ASME SB283 |
ASTM B124 |
ASTM B283 |
ASTM F467 |
ASTM F468 |
SAE J463 |
ASTM B150 |
SAE J461 |
The chemical composition of UNS C64200 copper alloy is outlined in the following.
Element |
Content (%) |
Aluminum, Al |
6.3-7.6 |
Silicon, Si |
1.5-2.2 |
Zinc, Zn |
0.5 |
Iron, Fe |
0.3 |
Nickel, Ni |
0.25 |
Tin, Sn |
0.2 |
Manganese, Mn |
0.1 |
Copper, Cu |
Remainder |