The following table shows the mechanical properties of UNS C64750 flat products as a function of heat treatment.
Temper |
Tensile Str. |
Elong. |
Shear Str. |
TF00 |
637 MPa (92 ksi) |
7% |
265 MPa (38 ksi) |
|
614 MPa (89 ksi) |
- |
- |
The chemical composition of UNS C64750 copper alloy is outlined in the following table.
Element |
Content (%) |
Nickel, Ni |
1.0-3.0 |
Iron, Fe |
1 |
Zinc, Zn |
1 |
Silicon, Si |
0.10-0.7 |
Magnesium, Mg |
0.1 |
Phosphorous, P |
0.1 |
Zirconium, Zr |
0.1 |
Tin, Sn |
0.05-0.8 |
Copper, Cu |
Remainder |
Copper and the elements mentioned in the above table together constitute 99.92% of this alloy.