Dec 13 2012
Bearing bronze UNS C93700 has a copper content of not less than 78%.
The following table shows the mechanical properties of UNS C93700 centrifugal cast alloy as a function of heat treatment.
Temper |
Tensile Str. |
Yield Str. |
Elong. |
M02 |
207MPa (30ksi) |
83MPa (12ksi) |
15% |
Equivalent materials to UNS C93700 copper alloy are the following:
- ASTM B30
- ASTM B505
- ASTM B584
- ASTM B763
- QQ C390
- SAE J461
- SAE J462
The chemical composition of UNS C93700 copper alloy is outlined in the following table.
Element |
Content (%) |
Copper, Cu |
78-82 |
Tin, Sn |
9-11 |
Lead, Pb |
8-11 |
Zinc, Zn |
0.8 |
Iron, Fe |
0.7 |
Nickel, Ni |
0.5 |
Antimony, Sb |
0.5 |
Phosphorous, P |
0.1 |
Sulfur, S |
0.08 |
Silicon, Si |
0.005 |
Aluminum, Al |
0.005 |