  • Article - 25 Jul 2013
    Pyromet CTX-909 alloy is a high-strength, precipitation hardenable superalloy that exhibits a low and relatively constant thermal expansion coefficient over a wide temperature range, good thermal...
  • Article - 24 Jul 2013
    Pyromet Alloy A-286 is an iron-base superalloy that offers high ductility in notched sections. It has higher notched rupture strength when compared to other commercial alloys with comparable high...
  • Article - 25 Jul 2013
    Pyromet CTX-3 alloy is a high strength, precipitation hardenable superalloy that exhibits low thermal expansion coefficient over a broad temperature range. It also possesses good thermal fatigue...
  • Article - 29 Jul 2013
    Rhenium is a silvery-white metal having one of the highest melting points of all metals. Being a member of group 7 of the periodic table, rhenium was the last stable element to be discovered in 1925.
  • Article - 23 Dec 2010
    Grinding-wheel loading can be defined as ground material either adhere to abrasive grains or become embedded in voids on a grinding-wheel surface.
  • Article - 11 Apr 2001
    Sialons are a family of ceramics consisting of silicon, aluminium, oxygen and nitrogen with applications in the automotive and matallurgical fields.

While we only use edited and approved content for Azthena answers, it may on occasions provide incorrect responses. Please confirm any data provided with the related suppliers or authors. We do not provide medical advice, if you search for medical information you must always consult a medical professional before acting on any information provided.

Your questions, but not your email details will be shared with OpenAI and retained for 30 days in accordance with their privacy principles.

Please do not ask questions that use sensitive or confidential information.

Read the full Terms & Conditions.