  • Article - 19 Nov 2012
    Super alloys have the capacity to function at very high temperatures and under extreme mechanical stress, and also where high surface stability is required. They consist of a number of elements in a...
  • Article - 15 Nov 2012
    Super alloys are also called high performance alloys. They have the capacity to function under very high temperatures and severe mechanical stress, and also where high surface stability is required.
  • Article - 23 Nov 2012
    Super alloys or high performance alloys contain a number of elements in a variety of combinations to achieve the desired result. They have good creep and oxidation resistance, and can be formed in...
  • Article - 15 Nov 2012
    Super alloys or high performance alloys are used at environments with very high temperature above 540ºC (1000ºF) where deformation resistance and high surface stability are chiefly required.
  • Article - 22 Nov 2012
    UNS C72800 has a copper content of not less than 82%.
  • Article - 27 Sep 2012
    Aluminum alloys are alloys having high electrical conductivity and strong corrosion resistance. These alloys tend to lose some of their strength at high temperatures ranging between 200 and 250°C (392...
  • Article - 13 Sep 2012
    Aluminum alloys have high electrical conductivity and strong corrosion resistance. These alloys tend to lose some of their strength at high temperatures ranging between 200 and 250°C (392 and 482°F).
  • Article - 27 Sep 2012
    Aluminum alloys are alloys having high electrical conductivity and strong corrosion resistance. These alloys tend to lose some of their strength at high temperatures ranging between 200 and 250°C (392...
  • Article - 27 Sep 2012
    Aluminum alloys have high electrical conductivity and strong corrosion resistance. They tend to lose some of their strength at elevated temperatures ranging between 200 and 250°C (392 and 482°F).
  • Article - 20 Sep 2012
    Aluminum alloys are alloys having high electrical conductivity and strong corrosion resistance. These alloys tend to lose some of their strength at high temperatures ranging between 200 and 250°C (392...

While we only use edited and approved content for Azthena answers, it may on occasions provide incorrect responses. Please confirm any data provided with the related suppliers or authors. We do not provide medical advice, if you search for medical information you must always consult a medical professional before acting on any information provided.

Your questions, but not your email details will be shared with OpenAI and retained for 30 days in accordance with their privacy principles.

Please do not ask questions that use sensitive or confidential information.

Read the full Terms & Conditions.