UNS C18143 high copper alloy has a copper content of not less than 99.6%.
The following table outlines the mechanical properties of UNS C18143 flat products as a function of heat treatment, measured at room temperature - 68o F (20o C).
Temper |
Tensile Str. |
Yield Str. |
Elong. |
H08 |
725 MPa (105 ksi) |
705 MPa (102 ksi) |
- |
|
650 MPa (94 ksi) |
600 MPa(87 ksi) |
2% |
|
575 MPa (83 ksi) |
530 MPa (76 ksi) |
- |