Sep 27 2012
The following table shows the mechanical properties of UNS C17455 rod as a function of heat treatment.
Temper |
Tensile Str. |
Elong. |
Rockwell |
B |
C |
F |
30T |
TH02 |
690MPa (100ksi) |
- |
93 |
- |
- |
- |
|
- |
15% |
- |
- |
- |
- |
The chemical composition of UNS C17455 copper alloy is outlined in the following.
Element |
Content (%) |
Nickel, Ni |
0.50-1 |
Zirconium, Zr |
0.5 |
Tin, Sn |
0.25 |
Lead, Pb |
0.20-0.60 |
Silicon, Si |
0.2 |
Iron, Fe |
0.2 |
Aluminum, Al |
0.2 |
Beryllium, Be |
0.15-0.50 |
Copper, Cu |
Balance |