Dec 20 2012
UNS C92500 has a copper content of not less than 85%.
The following table shows the mechanical properties of UNS C92500 continuous cast alloy as a function of heat treatment.
Temper |
Tensile Str. |
Yield Str. |
Elong. |
Fatigue Str. |
M01 |
276MPa (40ksi) |
165MPa (24ksi) |
10% |
- |
Equivalent materials to UNS C92500 copper alloy are provided below:
- ASTM B30
- ASTM B505
- QQ C390
- SAE J461
- SAE J462
The chemical composition of UNS C92500 copper alloy is outlined in the following table.
Element |
Content (%) |
Copper, Cu |
85-88 |
Tin, Sn |
10-12 |
Lead, Pb |
1.0-1.5 |
Nickel, Ni |
0.8-1.5 |
Zinc, Zn |
0.5 |
Phosphorus, P |
0.3 |
Iron, Fe |
0.3 |
Antimony, Sb |
0.25 |
Sulfur, S |
0.05 |
Aluminum, Al |
0.005 |
Silicon, Si |
0.005 |