New Record Set for Silicon Solar Cell Efficiency

SANYO Electric Co., Ltd. (SANYO) announced today it has broken its own record for the world's highest energy conversion efficiency in practical size (100 cm2 or more) crystalline silicon-type solar cells, achieving a efficiency of 23.0% (until now 22.3%) at a research level for its proprietary HIT solar photovoltaic cells.

Improving the quality of heterojunction of HIT solar cell

The structure of the HIT solar cell allows a possible reduction in recombination loss of the electrical element (charged carrier) by surrounding the energy generation layer of single thin crystalline silicon (c-Si) with high quality ultra-thin amorphous silicon (a-Si) layers. SANYO has recently managed to improve the quality of the HIT solar cell junction through developing a technology for depositing a higher quality a-Si layer over the c-Si substrate while protecting the c-Si surface from being damaged.

The result was an increase in the open circuit voltage (Voc) from 0.725V to 0.729V.

Reduction of optical absorption loss

In the solar cell, sunlight hitting the surface needs guidance to the c-Si, the energy generation layer, with the smallest possible absorption loss. For the HIT solar cell, reducing optical absorption loss in the a-Si layer, which covers the front and rear surfaces of the c-Si, and the transparent conductive layer was a challenge. Absorption of short-wavelength solar radiation by the a-Si layer and that of long-wavelength solar radiation by the transparent conductive layer were the causes of the optical absorption loss. SANYO has recently developed know-how to reduce optical absorption loss in both the a-Si and transparent conductive layers. As a result, the short circuit current (Isc) improved from 39.2mA/cm2 to 39.5mA/cm2.

Reduction of resistance loss

In the solar cell, generated electric current is collected and taken out through the surface grid electrode. SANYO recently realized lower-resistance electrode material for use in the grid electrode and a higher-aspect ratio through improving printing technology, leading to a success in reduction of resistance loss when an electric current flows through the grid electrode. As a result, the fill factor (FF) was improved from 0.791 to 0.80.

For the full release and all detailed information, click here

Tell Us What You Think

Do you have a review, update or anything you would like to add to this news story?

Leave your feedback
Your comment type
Submit

While we only use edited and approved content for Azthena answers, it may on occasions provide incorrect responses. Please confirm any data provided with the related suppliers or authors. We do not provide medical advice, if you search for medical information you must always consult a medical professional before acting on any information provided.

Your questions, but not your email details will be shared with OpenAI and retained for 30 days in accordance with their privacy principles.

Please do not ask questions that use sensitive or confidential information.

Read the full Terms & Conditions.