Dec 10 2012
High copper alloy UNS C18620 has a copper content of not less than 99.40%.
The following table shows the mechanical properties of UNS C18620 tubes as a function of heat treatment.
Temper |
Tensile Str. |
Elong. |
H04 |
355MPa (51ksi) |
- |
|
500MPa (72ksi) |
2% |
ANNEAL |
225MPa (363ksi) |
- |
|
300MPa (43ksi) |
40% |