Copper-Zinc-Alloy Rod and Bar UNS C28500 – Mechanical Properties

UNS C28500 copper-zinc-alloy has a copper content of not less than 57%.

The following table shows the mechanical properties of UNS C28500 rod and bar as a function of heat treatment.

Temper Tensile Str. Yield Str. Elong. Rockwell
B C F 30T
H80 600 MPa (73 ksi) 330 MPa (48 ksi) 20% 150 - - -
480 MPa (70 ksi) 300 MPa (44 ksi) - - - - -
650 MPa (80 ksi) 400 MPa (58 ksi) - - - - -

The chemical composition of UNS C28500 copper alloy is outlined in the following table.

Element Content (%)
Copper, Cu 57-59
Iron, Fe 0.35
Lead Pb 0.25
Zinc, Zn Balance

Tell Us What You Think

Do you have a review, update or anything you would like to add to this article?

Leave your feedback
Your comment type
Submit

While we only use edited and approved content for Azthena answers, it may on occasions provide incorrect responses. Please confirm any data provided with the related suppliers or authors. We do not provide medical advice, if you search for medical information you must always consult a medical professional before acting on any information provided.

Your questions, but not your email details will be shared with OpenAI and retained for 30 days in accordance with their privacy principles.

Please do not ask questions that use sensitive or confidential information.

Read the full Terms & Conditions.