Sep 27 2012
High copper alloy UNS C14750 has a copper content of not less than 99.6%.
The following table shows the mechanical properties of UNS C14750 rods, tubes and shapes as a function of heat treatment and thickness.
Temper |
Tensile Str. |
Yield Str. |
Elong. |
H04 |
220MPa (32ksi) |
50MPa (7ksi) |
- |
|
250MPa (36ksi) |
200MPa (29ksi) |
10% |
|
360MPa (52ksi) |
320MPa (46ksi) |
- |