Sep 27 2012
Phosphorus-deoxidized UNS C15715 has a copper content of not less than 99.62%.
Tabulated below are the mechanical properties of UNS C15715 rods as a function of heat treatment and thickness.
Temper |
Thickness |
Tensile Str. |
Elong. |
Rockwell |
B |
C |
F |
30T |
M30 |
28.6mm (1.125in) |
393MPa (57ksi) |
27% |
57 |
- |
- |
- |
O61 |
7mm (0.275in) |
407MPa (59ksi) |
24% |
63 |
- |
- |
- |