  • Article - 6 Aug 2012
    UNS C16500 copper has good corrosion resistance and moderate strength. C16500 copper is slightly stronger than C16200. The following datasheet will provide details about UNS C16500 copper including...
  • Article - 13 Nov 2012
    UNS numbers C10100 to C13000 indicate the types of pure copper. Pure and unalloyed copper has excellent corrosion resistance and high thermal and electrical conductivity. Unalloyed copper grades vary...
  • Article - 19 Sep 2012
    UNS C12100 copper alloys have improved embrittlement resistance during the welding process due to deoxidization.
  • Article - 3 Oct 2012
    UNS C11100 electrolytic tough pitch copper alloys are anneal resistant. The following datasheet covers the chemical composition, physical and mechanical properties, designations and fabrication and...
  • Article - 18 Sep 2012
    Copper nickel alloys are alloys that have moderate strength and thermal stability in high temperature levels. The high oxidation resistance of these alloys is visible in moist air and steam.
  • Article - 27 Sep 2012
    Temper designations for copper alloys and copper products are indicated by the standard ASTM B601. This standard defines the terminology of the processes responsible for the production of tempers and...
  • Article - 3 Oct 2012
    Bronzes are bearing materials comprising a wide range of properties derived from a variety of compositions and alloys. This data sheet will discuss the chemical composition, physical and mechanical...
  • Article - 27 Jul 2012
    Master Bond Supreme 10HT is a one component system formulated to withstand creep and fatigue due to high application stresses.
  • Article - 27 Jul 2012
    Master Bond Supreme 10AOHT represents a breakthrough in epoxy adhesive technology featuring a unique balance of performance properties for demanding bonding.
  • Article - 27 Jul 2012
    Master Bond Supreme 3HT-80 cures at 175°F (80°C) – well below the 250-300°F required by typical one component epoxies.

While we only use edited and approved content for Azthena answers, it may on occasions provide incorrect responses. Please confirm any data provided with the related suppliers or authors. We do not provide medical advice, if you search for medical information you must always consult a medical professional before acting on any information provided.

Your questions, but not your email details will be shared with OpenAI and retained for 30 days in accordance with their privacy principles.

Please do not ask questions that use sensitive or confidential information.

Read the full Terms & Conditions.